Selective Laser Sintering (SLS)
Made with Plastic/Elastomer Powder
Sample built layer by layer
Horizontal Slide with Fixed Vertical Movement
Filetype ‘.stl’ used - structural triangle language
Finished sample cools for 12-24 hrs then pulled out of Powder